Apple Watch pitting corrosion?


this apple watch bought in april 2016. love watch started noticing spots 6 months use. used think aluminium didn’t corrode. corrosion sweat?

[​img]

[​img]

[​img]
 

attached files:

have been using in pool or ocean?
 